a. The biggest variation is due to the shift from using D50 to D100.
b. The previous test procedure (RP13E) measured the distribution of the apertures in the screen.RP13C uses a physical and repeatable test using actual solids (dry aluminum oxide) which measures the coarsest particle that can pass through the screen.